Obtention of Li3xLa2/3−xTiO3 ceramics from amorphous nanopowders by spark plasma sintering

Ferroelectrics, 498 (2016) 62-66

In this work, Li3xLa2/3-xTiO3 powder with nominal lithium content (x = 0.08) was synthesized by mechano synthesis method. Spark plasma sintering (SPS) was employed to prepare lithium lanthanum titanium oxide solid-state ceramic. The techniques of X-ray diffraction, high resolution scanning electron microscopy, and Raman spectroscopy were used to characterize the composition and microstructure of samples. The results showed that fine-grained ceramics with relative density of 95.5% were obtained by sintering the oxide powders at 1100 degrees C for only 5min.