Nanoindentation of (Ti,Ta)(C,N)-Co cermets prepared by methods of mechanochemistry

International Journal of Refractory Metals & Hard Materials, 49 (2015) 219-224

Nanoindentation of (Ti,Ta)(C,N)-Co cermets prepared by methods of mechanochemistry

Four materials TixTa(1 – x)C(0.5)N(0.5)-20%Co of two chemical compositions (x = 0.9 and 0.95) and two high energy milling methods (one stage and two stage milling) have been prepared. Nano-hardness and elastic modulus for microstructure as a whole and for individual constituent phases (matrix and carbide grains) were obtained by instrumented indentation. Individual targeted indentations as well as grid nanoindentation technique were used to discern the individual constituents’ properties. Maximum loads of 20 mN for individual phases and 300 mN for composite microstructure were applied. Materials with higher amount of Ti had larger grains but the milling procedure had stronger influence on the grain size. The two step milling resulted in finer microstructures but with a much wider grain size distribution. Final composite mechanical properties, however, were very similar. Hardness and indentation elasticity modulus of all materials were comparable within the errors of measurement.

WhatsApp
X
LinkedIn
Email